Main usage |
For welding light vehicles, vehicles, general machines, thin plate structures of ships, and thick plate structures |
Properties |
CR-13 is a high titanium oxide type electrode with beautiful bead appearance, good slag removal property and easy to create repeated arc. As the depth of the weld penetration is shallow, it is suitable especially for welding ultra-thin plates and thick plate structures. |
Work procedure |
If applied excessively high current, x-ray performance may degrade, spatter may increase and undercut may form. Therefore, use within the proper current range. If the electrode absorbed moisture, dry for 30-60 minutes at 70-100℃ before use. |
Shielding gas |
- |